Technical guides

Specify with confidence.

Practical, independent guidance for architects, engineers, contractors and owners, covering the factors that determine how a paved surface performs over its life.

Guide 01

Thickness and strength.

Many pavements fail prematurely because they were selected on price and appearance alone. Service life is governed by two parameters, thickness and compressive strength, and both should be specified against the traffic the surface will carry.

UseTrafficThicknessTypical grade
Footpaths, gardens, courtyardsPeople only60 mmM30 to M35
Driveways, parking baysLight60 to 80 mmM35 to M40
Streets, fuel stations, commercial areasMedium80 mmM40 to M50
Bus terminals, yards, portsHeavy100 mm or moreM50 and above

What the numbers mean

The grade (M30, M40, M50) is the concrete’s compressive strength in N/mm². Strength stops the block crushing, and thickness spreads the load into the bed underneath. The two work together: a thick block of weak concrete fails as surely as a thin block of strong concrete.

Beyond compressive strength

A durable paver also requires low water absorption, tight dimensional tolerances for effective interlock, and high abrasion resistance. When evaluating suppliers, request test data for each of these properties, not a strength figure alone.

Rule of thumb: for any surface carrying regular vehicular traffic, specify no less than 80 mm and M40. The saving on thinner units is quickly lost to the cost of relaying.

Guide 02

Colour that endures.

Paving that fades from terracotta to grey within a few seasons is a familiar sight, and an avoidable one. Three manufacturing factors determine colour permanence.

A dedicated face layer

Quality coloured pavers are produced in two layers: a structural base and a dense, pigment-rich wearing surface. Lower-grade units disperse a small quantity of pigment through the entire body, producing weaker colour in an open-textured surface that weathers rapidly.

Pigment quality

Synthetic iron-oxide pigments are UV-stable minerals that resist bleaching; low-grade dyes do not. The difference is invisible on installation and unmistakable within a few years.

Controlled curing

Efflorescence, the white bloom sometimes seen on new paving, is caused by salts migrating to the surface during drying. Controlled curing minimises it, whereas sun-dried units bloom heavily and develop micro-cracking. Light efflorescence on any new concrete is natural and weathers away within months.

Three questions for any supplier: Is there a dedicated face layer? Which pigment is used? How are the units cured?

Guide 03

Permeable and grass paving.

Conventional paving seals the ground, converting monsoon rainfall into runoff that floods streets, overloads drains and bypasses the aquifers our towns depend on. Permeable systems allow rainwater to infiltrate where it falls.

How they work

Permeable pavers incorporate widened, aggregate-filled joints or drainage voids, laid over an open-graded stone reservoir that stores water as it infiltrates. Grass pavers form a load-bearing concrete grid with open cells for turf, creating green surfaces that still accommodate vehicles.

The benefits

Groundwater recharge, reduced peak runoff and cooler surface temperatures, together with support for rainwater-management requirements in building bye-laws and credits under green building ratings such as IGBC and GRIHA.

Which one where

Permeable pavers suit car parks, residential streets, walkways and plazas. Grass pavers suit occasional-traffic areas such as overflow parking, driveways, fire lanes and landscape margins. Both depend on a correctly engineered sub-base.

Design note: involve your supplier at design stage, before the BOQ is finalised. Joint fill and sub-base matter as much as the unit itself.

Have a technical question?

Share the application, expected traffic and design intent, and our team will advise.